Nanotechnology and construction: use of nanoindentation measurements to predict macroscale elastic properties of high strength cementitious composites

Auteur(s):


Médium: article de revue
Langue(s): anglais
Publié dans: Revista IBRACON de Estruturas e Materiais, , n. 3, v. 5
Page(s): 284-295
DOI: 10.1590/s1983-41952012000300002
Abstrait:

This paper aims to present the experimental results involving the use of nanoindentation measurements and prediction of macroscale elastic properties of high performance cementitious composites (HPCC). The elastic properties of HPCC mixture were evaluated at different length scales by nanoindentation (microscale), and elastic moduli and compressive strength tests (macroscale). The nanoindentation results, obtained by grid indentation with subsequent phase deconvolution, were complemented by an independent porosimetry test and inserted into a two-step analytical homogenization scheme to predict the overall macroscale properties. The final results show that the presented method allows a reliable advanced prediction of HPCC elastic properties indicating, thus, that inserting nanotechnology in the concrete industry can be promising, since it would allow the production of a more predictable composite in an easier and less expensive way.

Structurae ne peut pas vous offrir cette publication en texte intégral pour l'instant. Le texte intégral est accessible chez l'éditeur. DOI: 10.1590/s1983-41952012000300002.
  • Informations
    sur cette fiche
  • Reference-ID
    10413593
  • Publié(e) le:
    12.02.2020
  • Modifié(e) le:
    12.02.2020
 
Structurae coopère avec
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine